Reflow soldering / vapour phase
Reflow soldering is the predominant mass soldering process in electronics manufacturing. The solder paste, which has been previously printed or dispensed, is melted in hot air or a hot nitrogen atmosphere, thereby forming a material-bonded and conductive connection between the components and the printed circuit board. Vapour-phase soldering is the method of choice for heat-sensitive assemblies: instead of convection heat, it utilises the heat of condensation from an inert liquid. For both processes, the solder paste determines the outcome – in terms of wetting, voiding and long-term reliability.
Reflow soldering is the predominant mass soldering process used in electronics manufacturing. The solder paste, which has been previously printed or dispensed, is melted in hot air or in a hot nitrogen atmosphere, thereby bonding the components to the printed circuit board in a material-bonded and conductive manner. Vapour-phase soldering is the method used for heat-sensitive assemblies: instead of convection heat, it utilises the heat of condensation from an inert liquid. For both processes, the solder paste determines the outcome – in terms of wetting, voiding and long-term reliability.
Reflow soldering and vapour-phase soldering
In conventional reflow soldering, the solder paste is melted in hot air or in a hot N₂ atmosphere. In vapour-phase soldering (VPS), the vapour of inert fluoride liquids acts as the heat transfer medium – primarily Fluorinert FC-70 from 3M, which has a boiling point of 215 °C.
Convection reflow
The solder paste is melted in hot air or a hot nitrogen atmosphere. This is the predominant mass soldering process.
Characteristics
- Tried and tested, and widely used
- Soldering under nitrogen is possible
- Voids can be removed via a vacuum step
Vapour-phase soldering (VPS)
The vapour of an inert fluoride liquid acts as a heat transfer medium. The heat of condensation released during the transition from the vapour to the liquid phase is utilised – heat transfer is therefore faster than with convection reflow soldering.
Characteristics
- uniform temperature, no heat damage to the printed circuit board
- less overheating than with infrared reflow – flux residues are easier to remove
- the solder does not oxidise – a less active flux is sufficient
- uniform heating: small chips can be mounted beneath larger components
Disadvantages
- High cost of the inert liquid
- Risk of contamination from flux
- It is not possible to select individual components
Almit’s best-sellers for reflow soldering
Three Almit products are particularly in demand for reflow soldering and vapour phase soldering – the full range of products is listed below.
-
The L1 all-rounder among Almit solder pastes
GT(R)-SR
Optimal wetting on surfaces that are difficult to wet, excellent print image on the smallest structures, suitable for pin-in-paste.
Find out more
-
Halogen-free classic
NH-GE
Dual boost flux with two activators – can be used with the same soldering profile as a halogen-activated paste.
Find out more
-
Lead-free with perfect strength
SJM series
SJM-03 and SJM-40 melt between 210 and 227 °C – SJM-40 shows no cracking even after 2,000 thermal cycles.
Find out more
Voids – gaseous inclusions in the solder joint
Pores result in reduced thermal conductivity. In components with high electrical currents, the heat generated can no longer be adequately dissipated via the porous solder joint – this leads to high component temperatures and, ultimately, to reduced performance or component lifespan.
Why this matters
Life-support equipment, aircraft control systems and driver assistance systems in cars all have one thing in common: they must function with absolute reliability for many years. A prerequisite for this is a high-strength, virtually pore-free solder joint.
Two factors to consider
The first is the process technology – the vacuum stage following reflow. The second is the solder paste itself, with low-voiding formulations such as NH(LVA) and SUC-UI.
- NH(LVA) (L0) reduces voids whilst improving printability
- SUC-UI (L1) is designed to minimise voids
Read more in the expert reports.
Almit solder pastes for the reflow process
GT(R)-SR
Optimal wetting on a wide variety of surfaces, excellent print image on the smallest structures, suitable for pin-in-paste applications.
NH-GE
Current top recommendation amongst halogen-free pastes: dual boost activation, copes even with challenging reflow profiles.
| System | Class | Positioning |
|---|---|---|
| GT(R)-SR | L1 | Current top seller: optimum wetting, excellent print image, suitable for pin-in-paste |
| NH-GE | L0 | Top recommendation – halogen-free: dual boost activation, handles challenging reflow profiles |
| NH IMT | L0 | Halogen-free with the wetting behaviour of an L1 paste, THR-compatible |
| TM-HP | L1 | The tried-and-tested classic, with stable printing and reflow behaviour |
| NH(LVA) | L0 | Low Voiding: fewer voids, better printability |
| SUC-UI | L1 | Minimal voids, for reliable thermal and electrical bonding |
| TM-HP S | L1 | Low slumping: high dimensional stability of the print image, for fine structures |
| NH-GE(H) | L0 | NH-GE with increased viscosity for a particularly stable print image |
| MR-NH | L0 | For critical area ratios – see stencil printing |
| HM1 RMA | L1 | The tried-and-tested all-rounder for leaded reflow processes |
| HA2-RA | M1 | A leaded classic solution with powerful M1 activation |
| SNTP | L1 | Developed for package-on-package (PoP), grain size 5–15 µm |
| FS | L1 | For the finest solder powders (Type 5 and finer), optimised for soldering under nitrogen |
Flux content and grain size vary by system – the values for each item are listed in the solder paste classification and on the product pages.
From the industry standard down to 139 °C
Thirteen alloys cover the reflow range – from the low-melting SnBi alloy through the standard SAC305 to the high-temperature antimony alloys.
Eutectic alloys have a defined melting point rather than a melting range – their bar is therefore just a line. Leaded alloys are shown in light colour.
| Alloy | Composition | Melting range | Properties |
|---|---|---|---|
| LFM-48 (SAC305) | Sn-3.0Ag-0.5Cu | 217–220 °C | Industry standard, globally qualified |
| LFM-82 (SAC396) | Sn-3.9Ag-0.6Cu | 217–218 °C | Increased silver content, fatigue-resistant solder joints |
| LFM-14 | Sn-3.5Ag-0.7Cu | 217–218 °C | High-silver, high-strength joints |
| SJM-03 | Sn-0.3Ag-0.7Cu-2.0Bi | 210–225 °C | Low-silver, high long-term reliability |
| SJM-40 | Sn-4.0Ag-2.0Bi-3.0Sb | 221–227 °C | Highest long-term reliability, proven in aerospace and defence |
| LFM-34 | Sn-3.5Ag | 221 °C | Eutectic, high joint strength |
| LFM-90 (SAC107) | Sn-1.0Ag-0.7Cu | 217–224 °C | Low-silver, cost-optimised |
| LFM-65 | Sn-58Bi | 139 °C | Eutectic, low-melting |
| LFM-70 | Sn-3.5Ag-0.5Bi-8.0In | 194–206 °C | Indium-containing SABI alloy |
| LFM-57 | Sn-5Sb | 235–240 °C | High temperature, silver-free |
| LFM-74 | Sn-10Sb | 246–258 °C | High temperature, silver-free |
| Sn62 | Sn-2.0Ag-36.0Pb | 179–190 °C | Leaded, reduces silver leaching |
| Sn63 | Sn-37.0Pb | 183 °C | Classic eutectic leaded alloy |
Continue to the product ranges: lead-free and leaded solder paste, low-melting-point as well as silver-free and low-silver systems. For a classification of the classes, see Solder Paste Classification; for the alloys, see the Alloy Table.
Paste application precedes reflow
How the paste is applied to the printed circuit board helps determine the reflow result. Almit covers all three methods with suitable formulations.
- Stencil printing – the standard method
- Dispensing – with pinpoint accuracy via a needle
- Jet printing – stencil-free and contact-free
Reflow soldering and vapour phase soldering – a brief explanation
What is the difference between reflow soldering and vapour phase soldering?
In reflow soldering, the solder paste is melted in hot air or a hot nitrogen atmosphere. In vapour-phase soldering, the vapour of an inert fluoride liquid acts as a heat transfer medium; the heat of condensation released is utilised, resulting in faster heat transfer than with convection reflow soldering.
Why is vapour-phase soldering suitable for heat-sensitive components?
In the vapour phase, the temperature is uniform, which prevents heat damage to the printed circuit board. Overheating is less severe than with infrared reflow soldering.
Can a milder flux be used in vapour-phase soldering?
Yes. As the solder does not oxidise in the vapour phase, a less active flux can be used than is usually the case.
What are voids or pores in a solder joint?
Pores are gaseous inclusions in the solder joint. They reduce thermal conductivity; in components carrying high currents, heat can no longer be dissipated sufficiently, leading to high component temperatures and a shorter service life.
Which solder paste reduces voiding?
NH(LVA) is a halogen-free, low-voiding formulation (L0) that significantly reduces voids whilst also improving printability. SUC-UI (L1) is also designed to minimise voids.
Which solder paste does Almit recommend for the reflow process?
GT(R)-SR (L1) is currently the best-selling lead-free solder paste. Among the halogen-free systems, NH-GE (L0) with dual boost activation is currently the top recommendation.
Are there any reflow solder pastes for low process temperatures?
Yes. With the eutectic SnBi alloy LFM-65 (Sn-58Bi), the melting point is 139 °C. The indium-containing SABI alloy LFM-70 lowers the melting range to 194–206 °C.
Which reflow paste suits your requirements?
Surfaces, component mix, peak temperature and void requirements determine the choice. Speak to your Almit specialist advisor.