SJM-40W NH(IMT) Flux 11,5% (20-38µ) 0,5kg Dose/ Jar
SJM-40W NH(IMT)  Flux 11,5%  (20-38µ)  0,5kg Dose/ Jar

Roll over and scroll on image to zoom

SJM-40W NH(IMT) Flux 11,5% (20-38µ) 0,5kg Dose/ Jar
816 200 99

 Added To Shopping Cart



Dramatically improve heat resistance property of SAC base alloy Specially best for against crack on big chip devices. SJM-40 has same strength as SAC305 initial stage even after 2000 cycles.
Flux Classifiction
ROL0
Alloy
SJM-40W
Flux %
11.5
Powder Size
20-38µm
Weight
0.5kg
Package
0.5kg Jar
Flux
NH(MT)
Jar/Reel/Catridge
Jar
Alloy Metal
Sn-4,0Ag-2.0Bi-3.0Sb
Temperature
217° - 227°C