Haloing

To improve the adhesion of internal conductor patterns in multilayer printed circuit boards, the copper is pre-treated by oxidation to form a black oxide layer. However, this black oxide layer can be attacked by the hydrochloric acid used to metallise the drill holes, i.e. it can be reduced and detached. This results in a whitish or reddish copper oxide ring forming around the via, known as a ‘red ring’ or ‘pink ring’. This phenomenon is also referred to as red ring formation or ‘haloing’. This reduces the adhesion of the inner layers. In standard circuits, the effects are minor; however, the high trace density of today’s multilayer printed circuit boards and the large number of via holes with a diameter of 0.4 mm or less make this a serious problem. One solution is the ZM process, in which zinc and sulphuric acid are used to minimise red ring formation. The following reaction takes place:

Zn + H₂SO₄ → ZnSO₄ + 2H;

CuO (red ring) + 2H → Cu + H₂O

As zinc has a lower electrochemical potential than copper, it acts as a ‘sacrificial anode’ and dissolves before the copper oxide does, thereby protecting the latter from reduction. → Black oxide treatment