Brown oxide treatment
Depending on the requirements, the inner layers of multilayer printed circuit boards should have either a glossy or a matt finish. Each of these surface finishes has specific properties. The former have 1.) good wetting, 2.) corrosion resistance and 3.) low thermal discolouration, whereas the latter 1.) react well with synthetic resins and 2.) are difficult to detach. The chemical treatment of the copper is therefore adapted to the respective requirements. Brown oxide treatment is one of the methods used to finish glossy copper surfaces and, in particular, enhances adhesion to synthetic resins. Its name refers to the brown colouration that the copper acquires as a result. The oxidising agents used for this purpose are listed in the table below. → Red ring formation, black oxide treatment
Oxidising agents for brown oxide treatment
Composition Treatment parameters Duration of resistance to red ring formation Peel strength
pH_______________________(Temperature)___(Time)
Copper acetate 30 g/l 45 °C______4 mins 30 mins 0.8–1.2 kg/cm² 4.9
Barium sulphide 24 g/l
Ammonium sulphide 24 g/l
Copper sulphate 24 g/l
Oxidising agents for brown oxide treatment